A remarkable alloy additive that restores the fluidity, colour and brightness of old or scrap yellow gold before you cast it. Use to eliminate the porosity associated with casting old gold.
Add 5% to your gold, melt and stir. Flow temperature: 1950°F.
One jar casts up to 800 dwt of gold.